Fig. 5.3
Radioautographs of Alkyd Resin Coated Wood Before
Surface Removal
Fig. 5.4 Radioautographs of Fig. 5.3 Surfaces After Removal of
100 Microns (Left) and 290 Microns (Right)
100
Per Cent Removed
Les
:
80
60
40l—
Q
20
LL
30 60
|
90
120
Thickness Removed(u)
Fig. 5.5
150
1
180
210
|
240
Effect of Surface Removal in Decontamination of
Alkyd Resin Painted Wood
hy
CONFIDENTIAL — RESTRICTED DATA